Rotating-field annealing produced 1–5 nm crystals in iron-based soft magnetic alloys, combining 1.94 T saturation flux density with about 0.8 A/m coercivity. The laboratory result could support lower-loss power electronics, but component-level efficiency, production throughput and long-term reliability remain unproven.